INCOLOY alloy 825 (UNS N08825 / W.Nr. 2.4858 / NS142 / NiCr21Mo) is a nickel-iron-chromium alloy with additions of molybdenum, copper, and titanium. The alloy’s chemical composition, given in Table 1, is designed to provide exceptional resistance to many corrosive environments. The nickel content is sufficient for resistance to chloride-ion stress-corrosion cracking. The nickel, in conjunction with the molybdenum and copper, also gives outstanding resistance to reducing environments such as those containing sulfuric and phosphoric acids. The molybdenum also aids resistance to pitting and crevice corrosion. The alloy’s chromium content confers resistance to a variety of oxidizing substances such as nitric acid, nitrates and oxidizing salt. The titanium addition serves, with an appropriate heat treatment, to stabilize the alloy against sensitization to intergranular corrosion. The resistance of INCOLOY alloy 825 to general and localized corrosion under diverse conditions gives the alloy broad usefulness. Applications include chemical processing, pollution control, oil and gas recovery, acid production, pickling operations, nuclear fuel reprocessing, and handling of radioactive wastes. Applications for alloy 825 are similar to those for INCOLOY alloy 020.

Limiting Chemical Composition, % of INCOLOY alloy 825

Nickel  38.0-46.0
Iron  22.0 min.
Chromium  19.5-23.5
Molybdenum  2.5-3.5
Copper  1.5-3.0
Titanium  0.6-1.2
Carbon  0.05 max.
Manganese  1.0 max.         
Sulfur  0.03 max.
Silicon  0.5 max.
Aluminum  0.2 max

Application

Chemical Processing

Pollution-control

Oil and gas well piping

Nuclear fuel reprocessing

Components in Pickling equipment like heating coils, tanks, baskets and chains

Acid production


  • Previous:
  • Next:

  • The use and maintain of the sawblade

    ◎ The carbide tip of sawblade is very sharp, so process of using must be prevent the carbide tip.

    ◎ PeriodicaI cleaning and support the machine,the spindle’s running tolerance must be less than h7.

    ◎ The flanges must be parallel to each other,must be of the same diameter 1/3 of the sawblade’s diameter(formuIti—rip saw blade is 1/2.

    ◎ When instaIIion the sawbIade,it shaII be 5-6 teeth higher than board surface.

    ◎ Before operation,check the firmly of the sawblade,be sure nobody in front of the machine. Do not feed of operation check whether the machine is good for operaiton. Periodical check the function of the machine,the certicaI jump is less than ±0.02MM,and the flap is less than ±0.01.

    ◎ After continuous use,must be removed and cleaning the sawblade,get rid of the resin and sawdust of the sawblade of both sides.Other wise it would beinfluence the effect of using the sawblade.

    ◎ Deposit of the sawblade,must not be layer the sawblade,it is putted in the originaI package inside.

    The renovate of the sawbIade

    ◎ The renovate of the carbide sawblade While it no longer sharpen and the horizontaI piece coarseaess. The power of using sawblade machine obviously Increase. When process materiaI,the materiaI appearred burst. The carbide tip exhaust more than 0.02MM.

    ◎ For the renovate the sawblade,it shouId be grinding by the a formal company, so be sure the quality of the sawblade after renovating.